Polymer Property : Tensile Impact Strength = 154 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 154 kJ/m²

@Temperature 23.0 °C
73.3 ft-lb/in²

@Temperature 73.4 °F
DAM; Short specimen; ASTM D1822
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers