Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 1.46 J | 1.08 ft-lb | ASTM D5420 |
RheTech Products HP532-01 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: Close out panelSpeaker grilleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.46 J | 1.08 ft-lb | ASTM D5420 |
RheTech Products HP532-00 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Natural Applications: Interior trimCenter tail light bezelPackage trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 1.46 J | 1.08 ft-lb | ASTM D5420 |
RheTech Products HP507-01 38% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: IP structural componentsSpeaker housingsAutomotive interior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |