Polymer Property : Gardner Impact = 1.84 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 2.50 J
1.84 ft-lb
ASTM D3029
Buckeye Polymers BP RPP 2011 C Polypropylene, 20% Mineral Filled
Applications:Outdoor FurnitureCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized thr..
Gardner Impact 2.50 J
1.84 ft-lb
ASTM D3029
Buckeye Polymers BP RPP 1510 C Polypropylene, 15% Mineral Filled
Calcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized through the addition of UV packag..