Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 13.8 - 36.0 J | 10.2 - 26.6 ft-lb | Average value: 28.6 J Grade Count:10 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini.. |