Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 11.07 J | 8.167 ft-lb | ASTM D3029 |
Multibase Multi-Pro® 2510 XGW Polypropylene Mineral Filled, 27% by weight.Features:Gloss, HighForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |