Polymer Property : Gardner Impact = 11.1 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 15.0 J
11.1 ft-lb
ASTM D3029
Washington Penn PPC7UF0-Black Polypropylene, High Flow Copolymer
Injection Molding Grade. Heat Stabilized. Meets Ford ESH-M4D293-B Spec.Data provided by Washington Penn Plastic Co., Inc.