Polymer Property : Gardner Impact = 12.5074 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 12.5074 - 137.051 J

@Temperature -30.0 - -6.67 °C
9.22501 - 101.083 ft-lb

@Temperature -22.0 - 20.0 °F
Average value: 37.9 J Grade Count:17
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..