Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 20.8 - 20.8 J @Temperature -23.0 - -23.0 °C |
15.3 - 15.3 ft-lb @Temperature -9.40 - -9.40 °F |
Average value: 14.7 J Grade Count:1 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||