Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FRp256-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT1004-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-47UV Thermoplastic Polyolefin, UV Stabilized, AYNA Light Prairie Tan Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT4802-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT4802-690UVA Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT5100-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT5100-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT5100-04 Thermoplastic Polyolefin, UV Stabilized, White Applications: IP structural componentBody side moldingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D5420 |
RheTech Products FT7013-721UV Thermoplastic Polyolefin, UV Stabilized, XDV Dark Slate Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | |
Protective Coating PC-7® Epoxy Paste PC-7® is a tough job Epoxy formulation developed for maximum bonding power. Components A (grey) and B (black), when mixed, react to form a bond of good strength. PC-7® formulation provides exten.. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | |
Protective Coating PC-SuperEpoxy™ Translucent Epoxy Putty PC-SUPEREPOXY™ is a non-drip, thixotropic, translucent paste with unlimited uses in bonding, sealing, and as a filler for most materials. Unlike conventional liquid epoxies, PC-SUPEREPOXY™ can be.. |
|||
Gardner Impact | 18.0 J | 13.3 ft-lb | ASTM D3029 |
LyondellBasell Astryn SZ021-2 Polypropylene Copolymer, 20% Talc Key Features: medium melt flow, medium modulus, mineral-filled, utility grade polypropylene copolymer, good impact and stiffness balance, versatileApplications: inner door panels and seat supportsDe.. |
|||
Gardner Impact | 18.0 J @Thickness 3.17 mm, Temperature -28.9 °C |
13.2 ft-lb @Thickness 0.125 in, Temperature -20.0 °F |
Geometry GC; ASTM D5420 |
ExxonMobil AP3N Polypropylene Impact Copolymer Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos.. |