Mechanical Properties Metric English Comments
Gardner Impact 18.1 J
13.3 ft-lb
No Break at 18.1 J; ASTM D-3029
Multibase Multi-Flex® TPE D 4502 BLK
Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo..
Gardner Impact 18.1 J
13.3 ft-lb
No break; ASTM D5420-95
Multibase Multi-Flex® TPO D 4508 D 4508
This product is suitable for airbag enclosures and is based on polyolefins/kraton rubber, exhibiting good paintability and low temperature performance.Data provided by Multibase.
Gardner Impact 18.1 J

@Temperature -23.0 °C
13.3 ft-lb

@Temperature -9.40 °F
Gardner
Network Polymers NPP 25-2001
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Gardner Impact 18.1 J

@Temperature -30.0 °C
13.3 ft-lb

@Temperature -22.0 °F
Gardner
Network Polymers NPP 25-2102
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Gardner Impact 18.1 J

@Temperature -30.0 °C
13.3 ft-lb

@Temperature -22.0 °F
Method G, geometry GC; ASTM D5420
Pinnacle Polymers 2135 H Medium Impact Polypropylene Copolymer, Injection Molding Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Gardner Impact 18.1 J

@Temperature 23.0 °C
13.3 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Gardner Impact 18.1 J

@Temperature 23.0 °C
13.3 ft-lb

@Temperature 73.4 °F
ASTM D5420
Washington Penn Homopolymer Polypropylene 40% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Gardner Impact 18.1 J

@Thickness 3.17 mm,
Temperature -28.9 °C
13.3 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..
Gardner Impact 18.1 J
13.3 ft-lb
1.6 cm diamter tup, 0.32cm x 7.6cm x 7.6cm steel panel
3M Scotchkote™ 206N Fusion Bonded Epoxy Coating (Fluid Bed Grade)
3M Scotchkote Fusion-Bonded Epoxy Coating 206N (Fluid Bed Grade) is a one-part, heat curable, thermosetting epoxy coating designed for corrosion protection of metal. The epoxy is applied to preheate..
Gardner Impact 18.1 - 28.2 J
13.3 - 20.8 ft-lb
Average value: 23.0 J Grade Count:4
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..