Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 3.60 J | 2.66 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Gardner Impact | 3.60 J | 2.66 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Gardner Impact | 3.60 J | 2.66 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Gardner Impact | 3.60 J | 2.66 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Gardner Impact | 3.60 J | 2.66 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Gardner Impact | 3.60 J | 2.66 ft-lb | ASTM D5420 |
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman. |