Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 2.71164 - 18.5295 J @Temperature -30.0 - -5.56 °C |
2.00000 - 13.6667 ft-lb @Temperature -22.0 - 22.0 °F |
Average value: 14.7 J Grade Count:3 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Gardner Impact | 2.71164 - 2.71164 J @Temperature -5.56 - -5.56 °C |
2.00000 - 2.00000 ft-lb @Temperature 22.0 - 22.0 °F |
Average value: 2.71 J Grade Count:1 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |