Polymer Property : Gardner Impact = 2.73 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 3.70 J
2.73 ft-lb
reported as J/cm; ASTM D3029-GB, unpainted
Plaskolite Duraplex® SG-05 Sign Grade Acrylic Sheet, Impact Modified
Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc.