Mechanical Properties Metric English Comments
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420-93
Multibase Multi-Pro® 0710 C Brown Polypropylene
Data provided by Multibase.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products F4702-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Exterior door moldingsRigid bumper coversInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT1055-50 Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite
Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey
Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT2400-648UV Thermoplastic Polyolefin, UV Stabilized, 848 Black
Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal
Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT4702-527UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic
Applications: Exterior door moldingsRigid bumper coversBodyside claddings and fairingsAutomotive grillesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT4702-698UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black
Applications: Bumper trimExterior componentsDoor claddingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT4702-715UV Thermoplastic Polyolefin, UV Stabilized, ZSP Deep Grey
Applications: Exterior componentsGrillesBumper trimDoor componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White
Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey
Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products P257-00 Polypropylene Copolymer, Natural
Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products P257-01 Polypropylene Copolymer, Black
Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products UVFT2500-01 Thermoplastic Polyolefin, 90K Flexural Modulus, UV Stabilized, Black
Applications: Air damsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black
Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420-93
Multibase Multi-Pro® 5002 X White 50% Filler Content Polypropylene
Multi-Pro 5002 X White is an extrusion grade filled polypropylene that has good stiffness as well as excellent impact properties. It can be made in any color.Data provided by Multibase.
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D5420
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black
Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 20.3 J

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
Ineos Styrenics Avantra® 2710 High Impact Styrenic Polymer (Global)
Description: Avantra® 2710 is a high-impact grade of polystyrene with improved stress crack resistance, developed primarily for extrusion and thermoforming applications, especially for the refrig..
Gardner Impact 20.3 J
15.0 ft-lb
ASTM D2794
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene
Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje..
Gardner Impact 20.3 J

@Temperature 23.0 °C
15.0 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 180 mil