Polymer Property : Gardner Impact = 22.60 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 22.60 J
16.67 ft-lb
ASTM D3029
Multibase Multi-Pro® 2513 C Whirlpool White Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Gardner Impact 22.60 J
16.67 ft-lb
STP 2223
Network Polymers NPP 25-0202 C
Description: Copolymer Polypropylene, Clarified RandomInformation provided by Network Polymers Inc.
Gardner Impact 22.60 J
16.67 ft-lb
ASTM D3029
Multibase Multi-Pro® 5002 CU Natural Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingFeatures:Gloss, LowInformation provided by Multibase
Gardner Impact >= 22.60 J
>= 16.67 ft-lb
A. Schulman PP 1692 Polypropylene High Impact Copolymer
DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman.
Gardner Impact 22.60 J

@Temperature -30.0 °C
16.67 ft-lb

@Temperature -22.0 °F
ASTM D5420
A. Schulman PP 3457-01 Copolymer Polypropylene
DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a..
Gardner Impact >= 22.60 J
>= 16.67 ft-lb
A. Schulman PP 1692 Polypropylene High Impact Copolymer
DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman.
Gardner Impact 22.60 J

@Temperature -30.0 °C
16.67 ft-lb

@Temperature -22.0 °F
ASTM D5420
A. Schulman PP 3457-01 Copolymer Polypropylene
DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a..
Gardner Impact >= 22.60 J
>= 16.67 ft-lb
A. Schulman PP 1692 Polypropylene High Impact Copolymer
DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman.
Gardner Impact 22.60 J

@Temperature -30.0 °C
16.67 ft-lb

@Temperature -22.0 °F
ASTM D5420
A. Schulman PP 3457-01 Copolymer Polypropylene
DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a..
Gardner Impact >= 22.60 J
>= 16.67 ft-lb
A. Schulman PP 1692 Polypropylene High Impact Copolymer
DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman.
Gardner Impact 22.60 J

@Temperature -30.0 °C
16.67 ft-lb

@Temperature -22.0 °F
ASTM D5420
A. Schulman PP 3457-01 Copolymer Polypropylene
DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a..
Gardner Impact >= 22.60 J
>= 16.67 ft-lb
A. Schulman PP 1692 Polypropylene High Impact Copolymer
DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman.
Gardner Impact >= 22.60 J
>= 16.67 ft-lb
A. Schulman PP 1692 Polypropylene High Impact Copolymer
DescriptionPolypropylene PP 1692 is an exceptional high impact copolymer with high flow for appearance parts.Information provided by A. Schulman.
Gardner Impact 22.60 J

@Temperature -30.0 °C
16.67 ft-lb

@Temperature -22.0 °F
ASTM D5420
A. Schulman PP 3457-01 Copolymer Polypropylene
DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a..
Gardner Impact 22.60 J

@Temperature -30.0 °C
16.67 ft-lb

@Temperature -22.0 °F
ASTM D5420
A. Schulman PP 3457-01 Copolymer Polypropylene
DescriptionPolypropylene PP 3457-01 is a copolymer polypropylene combining high impact at cold temperatures while maintaining stiffness. Ideal for durables in such applications for the furniture, a..