Mechanical Properties Metric English Comments
Gardner Impact 25.0 J
18.4 ft-lb
ASTM D3029
LyondellBasell Hifaxâ„¢ CB189FC Thermoplastic Olefin Resin
Key Features: medium melt flow, medium high modulus, precolored thermoplastic olefin resin, good impact and stiffness balance, good dimensional stability, good processability, low foggingApplication..
Gardner Impact 25.0 - 35.0 J
18.4 - 25.8 ft-lb
SABIC Method
SABIC Innovative Plastics Noryl FN215D PPE+HIPS (Europe-Africa-Middle East)
NORYL FN215 is a Noryl Engineering structural foam grade fulfilling a wide range of application requirement. Moulded with the recommended blowing agents, this material provides all the performance r..
Gardner Impact 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D3029
LyondellBasell Hifax™ ETA-3163UV Thermoplastic Olefin Resin
Key Features: medium melt flow, medium high modulus, UV-stabilized thermoplastic olefin resin, excellent impact and stiffness balance, excellent weatherability, good processabilityApplications: mold..