Mechanical Properties Metric English Comments
Gardner Impact 1.47 - 33.9 J
1.08 - 25.0 ft-lb
Average value: 14.6 J Grade Count:21
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Gardner Impact 0.565 - 33.9 J
0.417 - 25.0 ft-lb
Average value: 5.46 J Grade Count:32
Overview of materials for Polypropylene with 10% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Talc Filler". Specific grades with primary filler content between 5% and 14% are ..