Mechanical Properties Metric English Comments
Gardner Impact 26.0 J

@Temperature 23.0 °C
19.2 ft-lb

@Temperature 73.4 °F
ASTM D5420
Flint Hills P5M4R-034 Polypropylene Random Copolymer
Features: Radiation resistant. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: medical devicesInformation Provided by Flint Hills Resources