Polymer Property : Gardner Impact = 30.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 30.0 J
22.1 ft-lb
ASTM D3029
LyondellBasell Astryn SD068-4 Polypropylene Copolymer, 40% Calcium Carbonate
Key Features: fractional melt flow, high modulus, mineral-filled, blow molding and extrusion grade polypropylene copolymer, good melt strength, excellent processability, excellent impact and stiffne..