Mechanical Properties Metric English Comments
Gardner Impact 43.4 J

@Temperature -28.9 °C
32.0 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene
DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat..
Gardner Impact 43.4 J

@Temperature -28.9 °C
32.0 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene
DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat..
Gardner Impact 43.4 J

@Temperature -28.9 °C
32.0 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene
DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat..
Gardner Impact 43.4 J

@Temperature -28.9 °C
32.0 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene
DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat..
Gardner Impact 43.4 J

@Temperature -28.9 °C
32.0 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene
DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat..
Gardner Impact 43.4 J

@Temperature -28.9 °C
32.0 ft-lb

@Temperature -20.0 °F
ASTM D3029
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene
DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat..
Copyright © lookpolymers.com All Rights Reserved