Mechanical Properties Metric English Comments
Gardner Impact 4.90 J
3.61 ft-lb
ASTM D5420-93
Multibase Multi-Flex® TPO D 5308-20 BLK
Glass reinforced TOP with improved stiffness and retention of low temperature resistance.Data provided by Multibase.
Gardner Impact 4.90 J - NB
3.61 ft-lb - NB
Average value: 56.5 J Grade Count:67
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v..