Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | >= 40.7 J @Temperature 22.8 °C |
>= 30.0 ft-lb @Temperature 73.0 °F |
ASTM D5420 |
Spartech PP7210 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Gardner Impact | >= 40.7 J @Temperature 22.8 °C |
>= 30.0 ft-lb @Temperature 73.0 °F |
ASTM D5420 |
Spartech PP7220 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Gardner Impact | >= 40.7 J @Temperature 22.8 °C |
>= 30.0 ft-lb @Temperature 73.0 °F |
ASTM D5420 |
Spartech PP7230 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Gardner Impact | >= 40.7 J @Temperature -28.9 °C |
>= 30.0 ft-lb @Temperature -20.0 °F |
|
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Gardner Impact | 40.7 J | 30.0 ft-lb | ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | 40.7 J @Temperature -28.9 °C |
30.0 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | 40.7 J | 30.0 ft-lb | ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Gardner Impact | >= 40.7 J @Temperature -28.9 °C |
>= 30.0 ft-lb @Temperature -20.0 °F |
|
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Gardner Impact | >= 40.7 J @Temperature -28.9 °C |
>= 30.0 ft-lb @Temperature -20.0 °F |
|
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | >= 40.7 J @Temperature -28.9 °C |
>= 30.0 ft-lb @Temperature -20.0 °F |
|
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | >= 40.7 J @Temperature -28.9 °C |
>= 30.0 ft-lb @Temperature -20.0 °F |
|
A. Schulman PP 1404-01 Polypropylene High Impact Polypropylene DescriptionPolypropylene PP 1404-01 is a medium flow, high-impact polypropylene for injection molded parts. Information provided by A. Schulman. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | >= 40.7 J @Temperature -28.9 °C |
>= 30.0 ft-lb @Temperature -20.0 °F |
|
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | 40.7 J | 30.0 ft-lb | ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | 40.7 J @Temperature -28.9 °C |
30.0 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | >= 40.7 J @Temperature -28.9 °C |
>= 30.0 ft-lb @Temperature -20.0 °F |
|
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | 40.7 J | 30.0 ft-lb | ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | 40.7 J @Temperature -28.9 °C |
30.0 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | >= 40.7 J @Temperature -28.9 °C |
>= 30.0 ft-lb @Temperature -20.0 °F |
|
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |
|||
Gardner Impact | 40.7 J | 30.0 ft-lb | ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | 40.7 J @Temperature -28.9 °C |
30.0 ft-lb @Temperature -20.0 °F |
ASTM D3029 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Gardner Impact | >= 40.7 J | >= 30.0 ft-lb | |
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 1407H-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 1407H-01 meets FDA Regulation 21 CFR 177.1520 for food contact .. |