Polymer Property : Gardner Impact = 5.649 J
Polymer Property :
Gardner Impact =
5.649 J
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Gardner Impact
5.649
J
4.167
ft-lb
ASTM D3029
Multibase Multi-Pro® 0710 C Black Polypropylene