Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 9.039 J | 6.667 ft-lb | ASTM D3029 |
Multibase Multi-Pro® 3012 RC Polypropylene Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |