Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Stiffness | 276 MPa | 40000 psi | ASTM D790 |
LyondellBasell Petrothene® NA216000 Low Density Polyethylene ApplicationsPETROTHENE NA 216-000 is a general purpose, heavy and medium weight coating resin, capable of coating weights down to 7.0 lbs/ream at line speeds of 1200 ft/min. It can be applied to pa.. |
|||
Flexural Stiffness | 276 MPa | 40000 psi | ASTM D790 |
LyondellBasell Petrothene® NA217000 Low Density Polyethylene ApplicationsPETROTHENE NA 217-000 is a high speed, lightweight coating resin for use with paper, films and other base stocks. This resin can yield coating weights down to 3.5 lbs/ream at line speed.. |