Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Stiffness | 827 MPa | 120000 psi | ASTM D747 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Flexural Stiffness | 827 MPa | 120000 psi | ASTM D747 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Flexural Stiffness | 827 MPa | 120000 psi | ASTM D747 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Flexural Stiffness | 827 MPa | 120000 psi | ASTM D747 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||
Flexural Stiffness | 827 MPa | 120000 psi | ASTM D747 |
A. Schulman LP479-01 High-Density Polyethylene Homopolymer DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In.. |
|||