Mechanical Properties Metric English Comments
Flexural Stiffness 6.40 MPa

@Temperature 23.0 °C
928 psi

@Temperature 73.4 °F
ASTM D474
Lubrizol Estane® 58610 Thermoplastic Polyurethane
Features: Combines flexibility, toughness and excellent roll release for calendering and melt coating applications.Uses: Injection molding and general extrusion techniques. It is used in film, shee..