Polymer Property : Ultimate Compressive Strength = 1714 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ultimate Compressive Strength 1714 MPa
248600 psi
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or ..