Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 107 J @Treatment Temp. 649 °C, Thickness 12.7 mm |
78.9 ft-lb @Treatment Temp. 1200 °F, Thickness 0.500 in |
Notch Position at Mid-Weld, aged for 2000h and tested at RT |
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Charpy Impact | 107 J @Temperature -73.3 °C |
79.0 ft-lb @Temperature -100 °F |
Notched |
ATI Wah Chang Nb/Nb Alloy C-103 This alloy satisfies most rocket engine applications for temperatures up to 2700°F because of superior mechanical properties at all temperatures. Offers weight savings over many rocket engine desig.. |