Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 151 J @Temperature 25.0 °C |
111 ft-lb @Temperature 77.0 °F |
No thermal exposure |
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |