Mechanical Properties Metric English Comments
Charpy Impact 17.6 J

@Tempering Temp. 593 °C
13.0 ft-lb

@Tempering Temp. 1100 °F
air cooled from 1850°F then tempered; V-notch
Crucible Steel CHRO-MOW® Tool Steel, AISI H12
Chro-Mow is a general purpose hot work tool steel, combining good high-temperature strength with moderate toughness and heat check resistance. It is suited for applications where drastic coolants ar..
Charpy Impact 17.6 J

@Tempering Temp. 538 °C
13.0 ft-lb

@Tempering Temp. 1000 °F
air cooled from 1850°F then tempered; V-notch
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11
Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su..
Charpy Impact 17.6 J

@Temperature 260 °C
13.0 ft-lb

@Temperature 500 °F
48-50 HRC; V-notch
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19
Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance..
Charpy Impact 17.6 J

@Temperature 98.9 °C
13.0 ft-lb

@Temperature 210 °F
V-notch
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum..
Charpy Impact 17.6 J

@Tempering Temp. 579.4 °C
13.0 ft-lb

@Tempering Temp. 1075 °F
air cooled from 1875°F then tempered; V-notch
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel
Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr..