Polymer Property : Charpy Impact = 174 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 174 J

@Treatment Temp. 593 °C,
Time 3.60e+6 sec
128 ft-lb

@Treatment Temp. 1100 °F,
Time 1000 hour
Room temp test after thermal exposure
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..