Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 48.8 J @Treatment Temp. 1120 °C |
36.0 ft-lb @Treatment Temp. 2050 °F |
austenitized; C-notch |
Crucible Steel CPM® 4V® Tool Steel CPM 4V is a powder metal tool steel with an outstanding combination of properties including high impact toughness and very good wear resistance. CPM 4V should be considered for service in fine blank.. |