Polymer Property : Charpy Impact = 43.4 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 43.4 J

@Tempering Temp. 316 °C
32.0 ft-lb

@Tempering Temp. 600 °F
hardened at 1475°F then tempered; C-notch
Crucible Steel KETOS® Tool Steel, AISI O1
Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording..
Charpy Impact 43.4 J

@Temperature 260 °C
32.0 ft-lb

@Temperature 500 °F
38 HRC; V-notch
Crucible Steel PEERLESS A Tool Steel, AISI H21
Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee..