Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 45.0 J @Temperature -20.0 °C |
33.2 ft-lb @Temperature -4.00 °F |
Typical |
Industeel CREUSABRO® 4000 High Wear Resistant Steel Description: CREUSABRO® 4000 is a high wear resistant steel, offering a 30 % extra in service life compared to a conventional 400 HB water quenched. Improved properties of CREUSABRO® 4000 resu.. |
|||
Charpy Impact | 45.0 J @Temperature -196 °C |
33.2 ft-lb @Temperature -321 °F |
Metal Sample from Plate Weld |
Haynes Hastelloy® C-2000® Nickel Alloy Shielded Metal Arc Welded (SMAW) All Weld Cruciform Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Charpy Impact | 45.0 J @Temperature -20.0 °C |
33.2 ft-lb @Temperature -4.00 °F |
Transverse |
ThyssenKrupp XABO® 355 T Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Charpy Impact | 45.0 J @Temperature -20.0 °C |
33.2 ft-lb @Temperature -4.00 °F |
Transverse |
ThyssenKrupp XABO® 460 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |