Mechanical Properties Metric English Comments
Charpy Impact 6.78 J

@Temperature 21.1 °C
5.00 ft-lb

@Temperature 70.0 °F
50 HRC; V-notch
Crucible Steel PEERLESS A Tool Steel, AISI H21
Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee..