Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 10.8 J

@Tempering Temp. 538 °C
8.00 ft-lb

@Tempering Temp. 1000 °F
air cooled from 1850°F then tempered; V-notch
Crucible Steel CHRO-MOW® Tool Steel, AISI H12
Chro-Mow is a general purpose hot work tool steel, combining good high-temperature strength with moderate toughness and heat check resistance. It is suited for applications where drastic coolants ar..
Charpy Impact 10.8 J

@Temperature 21.1 °C
8.00 ft-lb

@Temperature 70.0 °F
38 HRC; V-notch
Crucible Steel PEERLESS A Tool Steel, AISI H21
Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee..