Mechanical Properties Metric English Comments
Ball Indentation Hardness 71.0 MPa
10300 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 300 HI4 POM
High impact strength grade, high damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Ball Indentation Hardness 71.0 MPa
10300 psi
358 N/30s; ISO 2039
Borealis MB350WG Polypropylene Compound, Mineral Filled
MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic..