Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 73.0 MPa | 10600 psi | DIN 53456 |
Global PP-2300-SC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-thin walled parts, electrical appliancesInformation provided by Global Polymers Corporation. |
|||
Ball Indentation Hardness | 73.0 MPa | 10600 psi | DIN 53456 |
Global PP-2311-SC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-electronic appliances, wall panelsInformation provided by Global Polymers Corporation. |