Ball Indentation Hardness 127 MPa
18400 psi
ISO 2039-1
Nilit FRIANYL A63 HS-GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics