Polymer Property : Ball Indentation Hardness = 147 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 147 MPa
21300 psi
ISO 2039
GEHR Plastics PSU Polysulfone
Polysulfone shows great thermal stability. It possesses a high mechanical strength, very good dielectric properties and hydrolysis resistance and a high radiation resistance. PSU has a low notch imp..
Ball Indentation Hardness 147 MPa
21300 psi
value at 30 sec.; ISO 2039-1
CENTROPLAST CENTRODAL LF Polyoxymethylene conductive
This material is electrically conductive, with high mechanical strength and dimensional stability. Applications include structural components in potentially explosive areas, components for divertin..