Ball Indentation Hardness 100 - 175 MPa
14500 - 25400 psi
Average value: 149 MPa Grade Count:8
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Ball Indentation Hardness 70.0 - 175 MPa
10200 - 25400 psi
Average value: 140 MPa Grade Count:35
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..