Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 161 MPa | 23400 psi | ISO 2039-1 |
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 161 MPa | 23400 psi | ISO 2039-1 |
Nilit FRIANYL A63 KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 161 MPa | 23400 psi | H358/30; ISO 2039-1 |
Chi Mei Kibisan® PN-117C SAN High Clarity |