Mechanical Properties Metric English Comments
Ball Indentation Hardness 176 MPa
25500 psi
ISO 2039-1
Nilit FRIANYL A63 KF30 M2 Nylon 6.6 for injection molding, 30% short glass fiber reinforced and 2% molybdenum disulphide lubricated
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 176 MPa
25500 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 300 XEC1 POM
Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe ..
Ball Indentation Hardness 176 MPa
25500 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 300 DW POM
Tribological modified grade with combination of damping and wear reducing additives. Finished parts have low coefficient of friction and wear with reduction of acoustic emission during sliding.Infor..