Polymer Property : Ball Indentation Hardness = 26400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 182 MPa
26400 psi
ISO 2039-1
Nilit FRIANYL A63 KV40 Nylon 6.6 for injection molding, 40% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 182 MPa
26400 psi
ISO 2039-1
Nilit FRIANYL B63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Ball Indentation Hardness 182 - 202 MPa
26400 - 29300 psi
Average value: 189 MPa Grade Count:3
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Ball Indentation Hardness 182 MPa
26400 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 300 GB2 POM
10% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.