Ball Indentation Hardness 273 MPa
39600 psi
dry; ISO 2039-1
EMS-Grivory Grivory® BG-60 FC PA6-GF60
Product description: Grilon BG-60 FC is a heat stabilized PA6 injection molding grade with 60% glass fibers. Grilon BG-60 FC has the following important properties: Short cycle timesExcellent surfac..