Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 202 MPa | 29300 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 GF2 POM 10% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Ball Indentation Hardness | 202 MPa | 29300 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 500 GB6 POM 30% glass beads filled low viscosity grade with very high stiffness and hardness with lowered shrinkage combined with easy molding of complicated shapesInformation provided by Zakłady Azotowe w .. |