Mechanical Properties Metric English Comments
Ball Indentation Hardness 231 MPa
33500 psi
DIN 2039
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced
Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor..