Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 345 MPa | 50000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVX-65 H black 9915 PA*-GF65 Product description: Grivory GVX-65H black 9915 is a 65% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolya.. |
|||
Ball Indentation Hardness | 345 MPa | 50000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65 Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami.. |