Polymer Property : Ball Indentation Hardness = 45000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 130 - 310 MPa
18900 - 45000 psi
Average value: 254 MPa Grade Count:23
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Ball Indentation Hardness 130 - 310 MPa
18900 - 45000 psi
Average value: 195 MPa Grade Count:8
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..